jervisbay

Uploaded together

Discussed in these Forum posts:

stainless palm weedy
OK, anybody who's bored with fin construction details blame Keef, I'm doing this at his request.

Basil has sliced me up some more end grain palm, and it's seasoned a bit more since the first one I made, so is a bit lighter.
First thing to do is mark out fin profile.
Palm marked out with Gav's shaped stainless leading edge alongside




Then because the palm has very little cross grain strength, I laminate a layer of 4oz glass onto one face to hold it together while I cut it out and foil the other side.





Once the epoxy's set I can start shaping the first side, possibly get around to that tomorrow.
View topic
carbon twill
I'm thinking of doing some laminating with twill, but it seems to fray very easily around the edges. Has anyone heard of using hairspray to hold the twill in position while it's cut and laid in position for wetting out?
I've been using 93gsm for a fairly decent finish on some fins, but the carbon supplier has bought some cheap crap which doesn't laminate well at all and I'm unable to find 93 anywhere.